General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.65 g/cm³ Show Supplier Material materials with Densidad of 2.65 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.2 - 1.5 mm Show Supplier Material materials with Espesor of 0.2 - 1.5 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 114 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 114 [-] |
Elongación A50 | 23.0 °C | 1 % Show Supplier Material materials with Elongación A50 of 1 % |
Límite elástico | 23.0 °C | 320 MPa Show Supplier Material materials with Límite elástico of 320 MPa |
Módulo de cizallamiento | 23.0 °C | 27 GPa Show Supplier Material materials with Módulo de cizallamiento of 27 GPa |
Módulo elástico | 23.0 °C | 71 GPa Show Supplier Material materials with Módulo elástico of 71 GPa |
Resistencia a la tracción | 23.0 °C | 380 MPa Show Supplier Material materials with Resistencia a la tracción of 380 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 121 W/(m·K) Show Supplier Material materials with Conductividad térmica of 121 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.6E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.6E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.15 % Show Supplier Material materials with Cobre of 0.15 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.35 % Show Supplier Material materials with Hierro of 0.35 % |
Magnesio | 4 - 5 % Show Supplier Material materials with Magnesio of 4 - 5 % |
Manganeso | 0.2 - 0.5 % Show Supplier Material materials with Manganeso of 0.2 - 0.5 % |
Otro | 0.05 - 0.15 % Show Supplier Material materials with Otro of 0.05 - 0.15 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Wind energy: Nacelle coverings, rotor hub, stairs; Components: Heat shields, Access hatches, Spoilers, General tranportation | |
Brazing | Brazing is not recommended. | |
Corrosion properties | Excellent | |
Welding | Good | |
Workability | Very good in special (Lüder lines resistant) O temper. |