General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Densidad of 2.69 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 200 W/(m·K) Show Supplier Material materials with Conductividad térmica of 200 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3.3E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.3E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Hierro | 0.04 % Show Supplier Material materials with Hierro of 0.04 % |
Magnesio | 0.8 - 1.1 % Show Supplier Material materials with Magnesio of 0.8 - 1.1 % |
Manganeso | 0.03 % Show Supplier Material materials with Manganeso of 0.03 % |
Otro | 0.01 % Show Supplier Material materials with Otro of 0.01 % |
Silicona | 0.06 % Show Supplier Material materials with Silicona of 0.06 % |
Titanio | 0.01 % Show Supplier Material materials with Titanio of 0.01 % |
Zinc | 0.04 % Show Supplier Material materials with Zinc of 0.04 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Cosmetics: Cosmetics pieces; Automotive trim: Window frame, Marque badges | |
Brazing | Good | |
Corrosion properties | Excellent | |
Welding | Good | |
Workability | Good |