General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Densidad of 2.69 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.3 - 1.2 mm Show Supplier Material materials with Espesor of 0.3 - 1.2 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 3 % Show Supplier Material materials with Elongación A50 of 3 % |
Límite elástico | 23.0 °C | 120 MPa Show Supplier Material materials with Límite elástico of 120 MPa |
Módulo de cizallamiento | 23.0 °C | 26.5 GPa Show Supplier Material materials with Módulo de cizallamiento of 26.5 GPa |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa |
Resistencia a la tracción | 23.0 °C | 170 - 190 MPa Show Supplier Material materials with Resistencia a la tracción of 170 - 190 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Conductividad térmica of 138 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.9E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Hierro | 0.1 % Show Supplier Material materials with Hierro of 0.1 % |
Magnesio | 0.6 - 1 % Show Supplier Material materials with Magnesio of 0.6 - 1 % |
Manganeso | 0.03 % Show Supplier Material materials with Manganeso of 0.03 % |
Otro | 0.05 % Show Supplier Material materials with Otro of 0.05 % |
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % |
Zinc | 0.05 % Show Supplier Material materials with Zinc of 0.05 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels; Anodizing quality; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim, Window frame, Marque badges | |
Corrosion properties | Excellent | |
General machinability | Good | |
Welding | Good | |
Workability | Good |