General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.74 g/cm³ Show Supplier Material materials with Densidad of 2.74 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.06 - 0.2 mm Show Supplier Material materials with Espesor of 0.06 - 0.2 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 5 % Show Supplier Material materials with Elongación A50 of 5 % |
Límite elástico | 23.0 °C | 90 MPa Show Supplier Material materials with Límite elástico of 90 MPa |
Módulo de cizallamiento | 23.0 °C | 25 GPa Show Supplier Material materials with Módulo de cizallamiento of 25 GPa |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa |
Resistencia a la tracción | 23.0 °C | 110 - 170 MPa Show Supplier Material materials with Resistencia a la tracción of 110 - 170 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 190 - 210 W/(m·K) Show Supplier Material materials with Conductividad térmica of 190 - 210 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3.1E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.1E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % |
Hierro | 1.2 - 2 % Show Supplier Material materials with Hierro of 1.2 - 2 % |
Magnesio | 0.1 % Show Supplier Material materials with Magnesio of 0.1 % |
Manganeso | 0.3 - 1 % Show Supplier Material materials with Manganeso of 0.3 - 1 % |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Limited | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels; Electronic devices: Housing of devices; Heat exchangers: Fins, Heat exchangers, General applications; Tubes: Industrial tubes, Flexible tubes, Pipes; Insulation; Semi-rigid and corrugated: Pet food, Smooth wall; Components: Automotive fins, Heat exchangers | |
Corrosion properties | Limited | |
Welding | Good | |
Workability | Very Good |