General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.71 g/cm³ Show Supplier Material materials with Densidad of 2.71 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.08 - 0.2 mm Show Supplier Material materials with Espesor of 0.08 - 0.2 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación A50 | 23.0 °C | 18 % Show Supplier Material materials with Elongación A50 of 18 % | according to EN 485-2 |
Límite elástico | 23.0 °C | 30 - 70 MPa Show Supplier Material materials with Límite elástico of 30 - 70 MPa | according to EN 485-2 |
Módulo de cizallamiento | 23.0 °C | 25.73 GPa Show Supplier Material materials with Módulo de cizallamiento of 25.73 GPa | |
Módulo elástico | 23.0 °C | 68.6 GPa Show Supplier Material materials with Módulo elástico of 68.6 GPa | |
Resistencia a la tracción | 23.0 °C | 90 - 120 MPa Show Supplier Material materials with Resistencia a la tracción of 90 - 120 MPa | according to EN 485-2 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | 20-100°C |
Conductividad térmica | 23.0 °C | 201 W/(m·K) Show Supplier Material materials with Conductividad térmica of 201 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3E-8 - 3.5E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3E-8 - 3.5E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Hierro | 0.5 - 1 % Show Supplier Material materials with Hierro of 0.5 - 1 % |
Magnesio | 0.1 % Show Supplier Material materials with Magnesio of 0.1 % |
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % |
Silicona | 0.4 - 0.8 % Show Supplier Material materials with Silicona of 0.4 - 0.8 % |
Titanio | 0.05 % Show Supplier Material materials with Titanio of 0.05 % |
Zinc | 0.1 % Show Supplier Material materials with Zinc of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Interiors and ceilings: Sheets for mechanized panels; Furniture, Plinths, Blinds: Intermediate transformation/interior use; Heat exchangers: Fins, General applications; Tubes: Flexible tube, Pipes; Insulation; Closures: Long cups, Short cups, Easy open; Cosmetic: Cosmetic pieces; Pharmacy: Pharma and para-pharma; Semi-rigid and corrugated: Pet food, Smooth wall; Foil stock: Foil app | |
Corrosion properties | Moderated | |
Welding | Excellent | |
Workability | Excellent |