General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.72 g/cm³ Show Supplier Material materials with Densidad of 2.72 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.09 - 0.14 mm Show Supplier Material materials with Espesor of 0.09 - 0.14 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 14 % Show Supplier Material materials with Elongación A50 of 14 % |
Resistencia a la tracción | 23.0 °C | 75 - 110 MPa Show Supplier Material materials with Resistencia a la tracción of 75 - 110 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K |
Chemical properties
Property | Value |
---|---|
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % |
Cromo | 0.03 % Show Supplier Material materials with Cromo of 0.03 % |
Hierro | 1.1 - 1.7 % Show Supplier Material materials with Hierro of 1.1 - 1.7 % |
Magnesio | 0.01 % Show Supplier Material materials with Magnesio of 0.01 % |
Manganeso | 0.03 % Show Supplier Material materials with Manganeso of 0.03 % |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % |
Titanio | 0.05 % Show Supplier Material materials with Titanio of 0.05 % |
Zinc | 0.05 % Show Supplier Material materials with Zinc of 0.05 % |
Technological properties
Property | ||
---|---|---|
Application areas | Foil stock: Foil app | |
Workability | Excellent |