General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.73 g/cm³ Show Supplier Material materials with Densidad of 2.73 g/cm³ |
Medidas
Property | Value |
---|---|
Espesor | 0.08 - 0.2 mm Show Supplier Material materials with Espesor of 0.08 - 0.2 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 15 % Show Supplier Material materials with Elongación A50 of 15 % |
Límite elástico | 23.0 °C | 40 - 80 MPa Show Supplier Material materials with Límite elástico of 40 - 80 MPa |
Resistencia a la tracción | 23.0 °C | 110 - 150 MPa Show Supplier Material materials with Resistencia a la tracción of 110 - 150 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % |
Cromo | 0.2 % Show Supplier Material materials with Cromo of 0.2 % |
Hierro | 0.6 - 1.2 % Show Supplier Material materials with Hierro of 0.6 - 1.2 % |
Magnesio | 0.2 - 0.6 % Show Supplier Material materials with Magnesio of 0.2 - 0.6 % |
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % |
Silicona | 0.6 % Show Supplier Material materials with Silicona of 0.6 % |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Semi-rigid and corrugated: Smooth wall |