General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.15 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.15 [-] | max. |
Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 33 % Show Supplier Material materials with Elongación of 33 % | min. | for thickness 1.8-2 mm | Transverse, A80 |
34 % Show Supplier Material materials with Elongación of 34 % | min. | for thickness 2-3 mm | Transverse, A80 | |
40 % Show Supplier Material materials with Elongación of 40 % | min. A5.65√So | for thickness 3-8 mm | Transverse | |
Límite elástico | 180 - 290 MPa Show Supplier Material materials with Límite elástico of 180 - 290 MPa | for thickness 1.8-2 mm | Transverse |
180 - 270 MPa Show Supplier Material materials with Límite elástico of 180 - 270 MPa | for thickness 2-8 mm | Transverse | |
Resistencia a la tracción | 270 - 350 MPa Show Supplier Material materials with Resistencia a la tracción of 270 - 350 MPa | for thickness 1.8-8 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | max. |
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | max. |
Carbono | 0.06 % Show Supplier Material materials with Carbono of 0.06 % | max. |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | This is widely used for bending and drawing applications in general industry, building, the automotive industry and related sectors (e.g. oil sumps for industrial vehicles etc). ArcelorMittal's steels for cold forming and deep drawing applications display good or even excellent performance in all types of deep drawing processes, enabling the production of complex parts. Uncoated hot rolled steels for bending and deep drawing applications are suitable under certain conditions for food contact, as specified in the Regulation (EC) No. 1935/2004 and French standard NF A 36-714. Please contact us for further information on this subject. | |
Coating | Galvanisation: Class 1 | |
Other | ArcelorMittal provides guarantees for thicknesses greater than 11 mm. | |
Welding | The weldability (spot and arc welding) of ArcelorMittal's hot rolled steels for cold forming and deep drawing is equivalent to that of cold rolled steels of corresponding grades. |