Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | min. |
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Boro | 0.001 % Show Supplier Material materials with Boro of 0.001 % | max. |
Carbono | 0.015 - 0.06 % Show Supplier Material materials with Carbono of 0.015 - 0.06 % | |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | max. |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % | max. |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.15 - 0.35 % Show Supplier Material materials with Manganeso of 0.15 - 0.35 % | |
Niobio | 0.003 % Show Supplier Material materials with Niobio of 0.003 % | max. |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Titanio | 0.008 % Show Supplier Material materials with Titanio of 0.008 % | max. |
Vanadio | 0.005 % Show Supplier Material materials with Vanadio of 0.005 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Steels for re-rolling are suitable, after processing, for cold forming by bending, drawing etc. They are also suitable for surface coating, with the exception of enamelling. Various examples of applications include: | |
Coating | Galvanisation: Class 1 | |
Heat Treatment | Batch annealing |