Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Value | Comment |
---|---|---|
Bend allowance | 1 [-] Show Supplier Material materials with Bend allowance of 1 [-] | min. | Transverse | for thickness 1.5-16 mm |
Elongación | 23 % Show Supplier Material materials with Elongación of 23 % | min. | for thickness 1.5-2 mm | Transverse, A80 |
24 % Show Supplier Material materials with Elongación of 24 % | min. | for thickness 2-3 mm | Transverse, A80 | |
28 % Show Supplier Material materials with Elongación of 28 % | min. A5.65√So | for thickness 3-16 mm | |
Límite elástico | 200 - 360 MPa Show Supplier Material materials with Límite elástico of 200 - 360 MPa | for thickness 1.5-2 mm | Transverse |
200 - 340 MPa Show Supplier Material materials with Límite elástico of 200 - 340 MPa | for thickness 2-16 mm | Transverse | |
Resistencia a la tracción | 270 - 440 MPa Show Supplier Material materials with Resistencia a la tracción of 270 - 440 MPa | for thickness 1.5-16 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. |
Carbono | 0.02 - 0.1 % Show Supplier Material materials with Carbono of 0.02 - 0.1 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 0.15 - 0.5 % Show Supplier Material materials with Manganeso of 0.15 - 0.5 % | |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Structural forming grade which is well suited to applications requiring high reproducibility of processing performance (especially control of springback). | |
Chemical composition | The chemical properties given are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |