Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.15 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.15 [-] | max. |
Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 32 % Show Supplier Material materials with Elongación of 32 % | min. | for thickness 1.8-2 mm | Transverse, A80 |
32 % Show Supplier Material materials with Elongación of 32 % | min. | for thickness 2-3 mm | Transverse, A80 | |
37 % Show Supplier Material materials with Elongación of 37 % | min. A5.65√So | for thickness 3-13 mm | |
Límite elástico | 200 - 310 MPa Show Supplier Material materials with Límite elástico of 200 - 310 MPa | for thickness 1.8-2 mm | Transverse |
200 - 290 MPa Show Supplier Material materials with Límite elástico of 200 - 290 MPa | for thickness 2-6 mm | Transverse | |
Resistencia a la tracción | 300 - 380 MPa Show Supplier Material materials with Resistencia a la tracción of 300 - 380 MPa | for thickness 1.8-13 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | min. |
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | max. |
Boro | 0.002 - 0.005 % Show Supplier Material materials with Boro of 0.002 - 0.005 % | |
Carbono | 0.02 - 0.08 % Show Supplier Material materials with Carbono of 0.02 - 0.08 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Structural forming grade which is well suited to applications requiring high reproducibility of processing performance (especially control of springback). That is why the S200D AM FCE grade is especially suitable for applications such as compressor casings. | |
Chemical composition | The chemical properties given are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |