General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.18 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.18 [-] | max. |
Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23 % Show Supplier Material materials with Elongación of 23 % | min. | for thickness 1.5-2 mm | Transverse, A80 | |
24 % Show Supplier Material materials with Elongación of 24 % | min. | for thickness 2-3 mm | Transverse, A80 | ||
28 % Show Supplier Material materials with Elongación of 28 % | min. A5.65√So | for thickness 3-20 mm | ||
Energía de impacto Charpy | 20 °C | 27 J Show Supplier Material materials with Energía de impacto Charpy of 27 J | min. | for thickness 1.5-20 mm |
Límite elástico | 240 - 360 MPa Show Supplier Material materials with Límite elástico of 240 - 360 MPa | for thickness 1.5-2 mm | Transverse | |
240 - 340 MPa Show Supplier Material materials with Límite elástico of 240 - 340 MPa | for thickness 2-20 mm | Transverse | ||
Resistencia a la tracción | 360 - 430 MPa Show Supplier Material materials with Resistencia a la tracción of 360 - 430 MPa | for thickness 1.5-20 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.01 % Show Supplier Material materials with Aluminio of 0.01 % | min. |
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | max. |
Carbono | 0.02 - 0.12 % Show Supplier Material materials with Carbono of 0.02 - 0.12 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 0.6 % Show Supplier Material materials with Manganeso of 0.6 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Structural forming grade which is well suited to applications requiring high reproducibility of processing performance (especially control of springback). The S240D AM FCE grade is popular with Steel Service Centres, since it allows them to rationalise their supplies of deep drawable and structural steel. This grade is a versatile material for numerous applications in industry markets. | |
Chemical composition | The chemical properties given are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |