General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.25 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.25 [-] | max. |
Medidas
Property | Value |
---|---|
Dimensions | *Pickled products with thicknesses up to 15 mm may be delivered after prior agreement: please contact us. Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23 % Show Supplier Material materials with Elongación of 23 % | min. | for thickness < 3 mm | Transverse, A80 | |
24 % Show Supplier Material materials with Elongación of 24 % | min. | for thickness < 3 mm, A80 | ||
27 % Show Supplier Material materials with Elongación of 27 % | min. A5.65√So | for thickness 3-16 mm | Transverse | ||
28 % Show Supplier Material materials with Elongación of 28 % | min. A5.65√So | for thickness 3-16 mm | ||
Energía de impacto Charpy | -20 °C | 40 J Show Supplier Material materials with Energía de impacto Charpy of 40 J | min. | for thickness 6-16 mm |
Límite elástico | 315 - 395 MPa Show Supplier Material materials with Límite elástico of 315 - 395 MPa | for thickness < 16 mm | |
340 - 420 MPa Show Supplier Material materials with Límite elástico of 340 - 420 MPa | for thickness < 16 mm | Transverse | ||
Resistencia a la tracción | 415 - 495 MPa Show Supplier Material materials with Resistencia a la tracción of 415 - 495 MPa | for thickness < 16 mm | |
420 - 500 MPa Show Supplier Material materials with Resistencia a la tracción of 420 - 500 MPa | for thickness < 16 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.015 % Show Supplier Material materials with Aluminio of 0.015 % | min. |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | max. |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.7 % Show Supplier Material materials with Manganeso of 0.7 % | max. |
Niobio | 0.045 % Show Supplier Material materials with Niobio of 0.045 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Titanio | 0.15 % Show Supplier Material materials with Titanio of 0.15 % | max. |
Vanadio | 0.2 % Show Supplier Material materials with Vanadio of 0.2 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | High strength Amstrong® steels are used in a wide range of applications in transport (earth movers, trailers, agricultural and railroad machinery etc), profiling (racks etc) and building (cranes, safety barriers, light poles etc). Significant weight reductions can be achieved by using Amstrong® steels, especially for cranes and heavy vehicle trailers, thus allowing a larger payload. | |
Chemical composition | The chemical properties given are based on cast analysis data. | |
Coating | Galvanisation: Class 1 Suitability for hot-dip zinc coating is defined as per the requirements of EN ISO 14713-2 Table 1 and NFA 35-503. | |
Other | Toughness guarantee at -40°C: on request |