General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.4 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.4 [-] | max. |
Medidas
Property | Value |
---|---|
Dimensions | For mill finish, coils in thicknesses greater than 20 mm can also be produced. Please contact us. Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 15 % Show Supplier Material materials with Elongación of 15 % | min. | for thickness 1.5-2 mm | Transverse, A80 | |
16 % Show Supplier Material materials with Elongación of 16 % | min. | for thickness 2-2.5 mm | Transverse, A80 | ||
17 % Show Supplier Material materials with Elongación of 17 % | min. | for thickness 2.5-3 mm | Transverse, A80 | ||
21 % Show Supplier Material materials with Elongación of 21 % | min. A5.65√So | for thickness 3-20 mm | Transverse | ||
Energía de impacto Charpy | -20 °C | 27 J Show Supplier Material materials with Energía de impacto Charpy of 27 J | min. | for thickness 6-20 mm |
Límite elástico | 265 MPa Show Supplier Material materials with Límite elástico of 265 MPa | min. | for thickness 16-20 mm | Transverse | |
275 MPa Show Supplier Material materials with Límite elástico of 275 MPa | min. | for thickness 1.5-16 mm | Transverse | ||
Resistencia a la tracción | 410 - 560 MPa Show Supplier Material materials with Resistencia a la tracción of 410 - 560 MPa | for thickness 3-20 mm | Transverse | |
430 - 580 MPa Show Supplier Material materials with Resistencia a la tracción of 430 - 580 MPa | for thickness 1.5-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | min. |
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.18 % Show Supplier Material materials with Carbono of 0.18 % | max. |
Cobre | 0.55 % Show Supplier Material materials with Cobre of 0.55 % | max. |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Nitrógeno | 0.012 % Show Supplier Material materials with Nitrógeno of 0.012 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Chemical composition | The above chemical properties are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |