Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 21 % Show Supplier Material materials with Elongación of 21 % | min. | for thickness 0.5-0.7 mm | A80 | Transverse |
22 % Show Supplier Material materials with Elongación of 22 % | min. | for thickness 0.5-0.7 mm | A80 | |
23 % Show Supplier Material materials with Elongación of 23 % | min. | for thickness 0.7-3 mm | A80 | Transverse | |
24 % Show Supplier Material materials with Elongación of 24 % | min. | for thickness 0.7-3 mm | A80 | |
Límite elástico | 280 - 360 MPa Show Supplier Material materials with Límite elástico of 280 - 360 MPa | for thickness 0.5-3 mm |
300 - 380 MPa Show Supplier Material materials with Límite elástico of 300 - 380 MPa | for thickness 0.5-3 mm | Transverse | |
Resistencia a la tracción | 370 - 470 MPa Show Supplier Material materials with Resistencia a la tracción of 370 - 470 MPa | for thickness 0.5-3 mm |
380 - 480 MPa Show Supplier Material materials with Resistencia a la tracción of 380 - 480 MPa | for thickness 0.5-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.015 % Show Supplier Material materials with Aluminio of 0.015 % | min. |
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.12 % Show Supplier Material materials with Carbono of 0.12 % | max. |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Manganeso | 1.4 % Show Supplier Material materials with Manganeso of 1.4 % | max. |
Niobio | 0.09 % Show Supplier Material materials with Niobio of 0.09 % | max. |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Titanio | 0.15 % Show Supplier Material materials with Titanio of 0.15 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The steel grade is particularly suitable for structural parts that do not require severe forming (profiling, bending or light drawing): automotive structures and reinforcements, industrial shelving systems, radiators, racking systems, furniture, mechanical engineering applications etc. | |
Surface condition | Surface cleanliness If improved surface cleanliness is required, ArcelorMittal also offers this steel grade with compulsory use of continuous annealing or hydrogen annealing. | |
Welding | Based on many years’ practical experience in arc and resistance spot welding of its products, ArcelorMittal can provide valuable technical assistance in defining the welding parameters for this grade. | |
Workability | Forming limit curves can be used to define the maximum strains not to be exceeded when forming steel by various methods, so as to avoid the risk of incipient necking. These curves are available on request. Please contact for other forming data on this grade for particular sheet thicknesses. |