Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 36 % Show Supplier Material materials with Elongación of 36 % | min. | for thickness 0.5-0.7 mm | Transverse | A80 |
38 % Show Supplier Material materials with Elongación of 38 % | min. | for thickness 0.7-2 mm | Transverse | A80 | |
Límite elástico | 140 - 230 MPa Show Supplier Material materials with Límite elástico of 140 - 230 MPa | for thickness 0.5-0.7 mm | Transverse |
140 - 210 MPa Show Supplier Material materials with Límite elástico of 140 - 210 MPa | for thickness 0.7-2 mm | Transverse | |
Resistencia a la tracción | 270 - 350 MPa Show Supplier Material materials with Resistencia a la tracción of 270 - 350 MPa | for thickness 0.5-2 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.06 % Show Supplier Material materials with Aluminio of 0.06 % | max. |
Carbono | 0.004 % Show Supplier Material materials with Carbono of 0.004 % | max. |
Manganeso | 0.4 % Show Supplier Material materials with Manganeso of 0.4 % | max. |
Silicona | 0.03 % Show Supplier Material materials with Silicona of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Solfer® grades are particularly suitable for the manufacture of casing panels for domestic appliances (hobs, covers, control panels, side panels etc) and for kitchen utensils (pots and pans). They can also be used for architectural applications, thanks to their excellent resistance to deformation during enamel firing. | |
Chemical composition | The manufacturing conditions guarantee very good resistance to "fish scale” defects (TH > 100 in accordance with EN 10209:2013). | |
Coating | Direct-on enamelling process: Solfer® and Solfer®+ grades Surface preparation: Surface preparation before enamelling must be performed with the greatest care (degreasing, pickling and coating with nickel). This is essential to achieve a good surface appearance of the part after enamelling and good adhesion of the enamel. The level of iron loss after pickling and the quantity of nickel deposited must therefore be monitored very precisely. Application of the enamel and firing: The thickness of the enamel layer deposited is generally about 130 microns. Moreover, Solfer® and Solfer®+ grades are compatible with all the common enamelling processes: wet spraying, electrostatic liquid or powder deposition. Taking into account its limited Al content, the Solfer® grade is particularly suitable for the ETE application process. Where wet application is used, it is imperative to dry the enamel layer before firing. Finally, firing is performed at a temperature of about 830°C. Two-coat / one-fire enamelling process: Solfer® CA, Solfer® and Solfer®+ grades Surface preparation: Enamel application and firing:
Finally, firing is performed at a temperature of about 830°C | |
Joining | Solfer® grades can easily be welded, whatever the welding process may be. Other joining processes (clinching, crimping) may also be used. | |
Processing methods | Solfer® grades can be formed by bending, profiling or deep drawing. |