Medidas
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 25 % Show Supplier Material materials with Elongación of 25 % | min. | for thickness 1.5-3 mm | Transverse | before enamelling, A80 |
30 % Show Supplier Material materials with Elongación of 30 % | min. A5.65√So | for thickness 3-6 mm | before enamelling | Transverse | |
Límite elástico | 260 - 420 MPa Show Supplier Material materials with Límite elástico of 260 - 420 MPa | for thickness 3-5 mm | Transverse | before enamelling |
280 - 420 MPa Show Supplier Material materials with Límite elástico of 280 - 420 MPa | for thickness 1.5-3 mm | Transverse | before enamelling | |
Resistencia a la tracción | 360 - 500 MPa Show Supplier Material materials with Resistencia a la tracción of 360 - 500 MPa | for thickness 1.5-6 mm | Transverse | before enamelling |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Boro | 0.004 % Show Supplier Material materials with Boro of 0.004 % | max. |
Carbono | 0.03 - 0.1 % Show Supplier Material materials with Carbono of 0.03 - 0.1 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Manganeso | 0.2 - 0.6 % Show Supplier Material materials with Manganeso of 0.2 - 0.6 % | |
Titanio | 0.04 % Show Supplier Material materials with Titanio of 0.04 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Hot rolled steel for one-side enamelling are mainly intended for the manufacture of tanks for water heaters. It can also be used for enamelled tubes or coiled pipes. | |
Coating | Surface preparation and enamelling of water heaters The surface must be treated by pickling or shot blasting. Enamel can be applied in a wet or dry process. Firing is performed at a temperature of about 830°C. The mechanical properties of hot rolled steel for one-side enamelling remain unchanged after forming and firing of the enamel. This offers the following advantages: | |
Processing methods | Forming of hot rolled grades for one-side enamelling presents no particular problems: All the usual welding processes can be used (TIG, MIG, seam welding, laser). |