General
Property | Value |
---|---|
Densidad | 7.6 g/cm³ Show Supplier Material materials with Densidad of 7.6 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Vickers | 205 - 235 [-] Show Supplier Material materials with Dureza Vickers of 205 - 235 [-] | Typical values |
Elongación | 15 % Show Supplier Material materials with Elongación of 15 % | min. | Guaranteed | Transverse | A80 |
20 - 30 % Show Supplier Material materials with Elongación of 20 - 30 % | Typical values | Transverse | A80 | |
Límite elástico | 480 MPa Show Supplier Material materials with Límite elástico of 480 MPa | min. | Guaranteed | Transverse |
495 - 545 MPa Show Supplier Material materials with Límite elástico of 495 - 545 MPa | Typical values | Transverse | |
Resistencia a la tracción | 590 MPa Show Supplier Material materials with Resistencia a la tracción of 590 MPa | min. | Guaranteed | Transverse |
610 - 660 MPa Show Supplier Material materials with Resistencia a la tracción of 610 - 660 MPa | Typical values | Transverse | |
Yield to strength ratio | 0.8 - 0.85 [-] Show Supplier Material materials with Yield to strength ratio of 0.8 - 0.85 [-] | Typical values |
Magnético
Technological properties
Property | ||
---|---|---|
Application areas | High strength values, combined with low losses and good permeability, make this grade particularly suitable for high-speed rotating machines. | |
Coating | This standard grade is available non-insulated or varnished with any of the coating types described in the following link https://industry.arcelormittal.com/catalogue/D28/EN . | |
Other | The above properties are obtained without heat treatment after stamping. The material as supplied possesses all the required magnetic properties. |