Mecánica
Property | Value | Comment |
---|---|---|
Dureza Vickers | 115 - 125 [-] Show Supplier Material materials with Dureza Vickers of 115 - 125 [-] | |
Elongación | 23 - 35 % Show Supplier Material materials with Elongación of 23 - 35 % | Typical values | Transverse | A80 |
Límite elástico | 270 - 370 MPa Show Supplier Material materials with Límite elástico of 270 - 370 MPa | min. | Guaranteed | Transverse |
290 - 370 MPa Show Supplier Material materials with Límite elástico of 290 - 370 MPa | Typical values | Transverse | |
Resistencia a la tracción | 270 - 370 MPa Show Supplier Material materials with Resistencia a la tracción of 270 - 370 MPa | Typical values | Transverse |
310 - 380 MPa Show Supplier Material materials with Resistencia a la tracción of 310 - 380 MPa | min. | Guaranteed | Transverse | |
Yield to strength ratio | 0.85 [-] Show Supplier Material materials with Yield to strength ratio of 0.85 [-] | min. | Guaranteed |
0.9 [-] Show Supplier Material materials with Yield to strength ratio of 0.9 [-] | min. | Typical values |
Technological properties
Property | ||
---|---|---|
Application areas | The Easy Punch grade is designed for small machines for intermittent use: | |
Coating | This Easy Punch grade is available non-insulated. Corrosion protection can be enhanced by applying a light oiling treatment. | |
Other | Usually, the client does not perform heat treatment after punching. Heat treatment is an option to increase the magnetic performance of Easy Punch. The Easy Punch grade is available in thicknesses ranging from 0.5 to 1.2 mm. For thicknesses less than 0.7 mm, the width may not exceed 1400 mm. |