Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 12 % Show Supplier Material materials with Elongación of 12 % | min. A5.65√So | for thickness 4 mm | Transverse and Longitudinal |
Límite elástico | 700 MPa Show Supplier Material materials with Límite elástico of 700 MPa | min. | for thickness 4 mm | Transverse/Longitudinal |
Resistencia a la tracción | 750 - 900 MPa Show Supplier Material materials with Resistencia a la tracción of 750 - 900 MPa | for thickness 4 mm | Transverse/Longitudinal |
Magnético
Technological properties
Property | ||
---|---|---|
Application areas | Hot rolled pole sheet grade can be supplied in the form of coils or sheets. It is designed for large high-speed machines because of their excellent combination of mechanical strength and good magnetic performance. Good magnetic properties are of major importance for the performance of the poles, whereas excellent mechanical properties are needed for the rims. | |
Coating | Hot rolled pole sheet grade is available non-insulated. It can be supplied with the hot rolled oxide layer or pickled. When pickled, they are protected with Easyfilm® dry coating, which offers protection against atmospheric corrosion for a period of three months | |
Other | These properties are obtained without heat treatment, whatever be the mechanical or thermal cutting process used to obtain the desired lamination diameter. The material as supplied possesses all the required magnetic properties. |