Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 19 % Show Supplier Material materials with Elongación of 19 % | min. | for thickness 5-120 mm | A8 | Transverse |
23 % Show Supplier Material materials with Elongación of 23 % | min. | for thickness 5-120 mm | A2 | Transverse | |
Límite elástico | 240 MPa Show Supplier Material materials with Límite elástico of 240 MPa | min. | for thickness 5-120 mm | Transverse |
Resistencia a la tracción | 450 - 585 MPa Show Supplier Material materials with Resistencia a la tracción of 450 - 585 MPa | for thickness 5-120 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. | for thickness 5-80 mm |
Carbono | 0.24 % Show Supplier Material materials with Carbono of 0.24 % | max. | for thickness 5-25 mm |
0.26 % Show Supplier Material materials with Carbono of 0.26 % | max. | for thickness 25-50 mm | |
0.28 % Show Supplier Material materials with Carbono of 0.28 % | max. | for thickness 50-80 mm | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. | for thickness 5-80 mm |
Manganeso | 0.85 - 1.2 % Show Supplier Material materials with Manganeso of 0.85 - 1.2 % | for thickness 5-80 mm |
Silicona | 0.15 - 0.4 % Show Supplier Material materials with Silicona of 0.15 - 0.4 % | for thickness 5-80 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Steel for pressure vessels are mainly used to manufacture boilers, drums, pressure or steam piping, industrial thermal vessels and heat exchangers. These steels are suitable for mechanical forming and welding. | |
Chemical composition | Manganese note: For each reduction by 0.01 percentage points below the specified maximum for carbon, an increase of 0.06 percentage points above the specified maximum for manganese is permitted, up to a maximum of 1.5% by heat analysis, and 1.6% by product analysis. | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). | |
Other | Available options Options available (after previous agreement): |