Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 22 % Show Supplier Material materials with Elongación of 22 % | min. A5.65√So | for thickness 5-100 mm | Transverse | |
Energía de impacto Charpy | -20 °C | 20 J Show Supplier Material materials with Energía de impacto Charpy of 20 J | min. | for thickness 5-50 mm | Transverse |
-20 °C | 24 J Show Supplier Material materials with Energía de impacto Charpy of 24 J | min. | for thickness 50-70 mm | Transverse | |
-20 °C | 27 J Show Supplier Material materials with Energía de impacto Charpy of 27 J | min. | for thickness 5-50 mm | |
-20 °C | 27 J Show Supplier Material materials with Energía de impacto Charpy of 27 J | min. | for thickness 70-100 mm | Transverse | |
-20 °C | 34 J Show Supplier Material materials with Energía de impacto Charpy of 34 J | min. | for thickness 50-70 mm | |
-20 °C | 41 J Show Supplier Material materials with Energía de impacto Charpy of 41 J | min. | for thickness 70-100 mm | |
Límite elástico | 235 MPa Show Supplier Material materials with Límite elástico of 235 MPa | min. | for thickness 5-100 mm | Transverse | |
Resistencia a la tracción | 400 - 520 MPa Show Supplier Material materials with Resistencia a la tracción of 400 - 520 MPa | for thickness 5-100 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | min. |
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % | max. |
Carbono | 0.21 % Show Supplier Material materials with Carbono of 0.21 % | max. |
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % | max. |
Cromo | 0.2 % Show Supplier Material materials with Cromo of 0.2 % | max. |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 0.6 % Show Supplier Material materials with Manganeso of 0.6 % | min. |
Molibdeno | 0.08 % Show Supplier Material materials with Molibdeno of 0.08 % | max. |
Níquel | 0.4 % Show Supplier Material materials with Níquel of 0.4 % | max. |
Otro | 0.12 % Show Supplier Material materials with Otro of 0.12 % | max. | Nb + Ti + V |
Technological properties
Property | ||
---|---|---|
Application areas | Steel for shipbuilding can be used for the entire range of shipbuilding applications e.g. for the hull and interior of ships | |
Chemical composition | For D grade, the carbon + 1/6 of the manganese content should not exceed 0.40%. The steel should contain aluminium, niobium, vanadium or other suitable grain-refining elements, either singly or in any combination. When these elements are used singly, the steel should contain the specified minimum content of the grain-refining element (0.02% ≤ Nb ≤ 0.05%, 0.05% ≤ V ≤ 0.10%, Ti ≤ 0.02%). When used in combination, the specified minimum content of each element is not applicable. | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). | |
Other | Agreements The maximum thickness approved in shipbuilding specifications can be communicated on request by your sales agent. Available options Options available (after prior agreement): Mechanical properties Charpy V notch impact test specimens should be taken in the longitudinal direction. Transverse test specimens are not usually required. Transverse test results for plates and wide flats should be guaranteed by the supplier. |