General
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.38 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.38 [-] | max. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 21 % Show Supplier Material materials with Elongación of 21 % | min. A5.65√So | for thickness 5-100 mm | Transverse | |
Energía de impacto Charpy | -20 °C | 24 J Show Supplier Material materials with Energía de impacto Charpy of 24 J | min. | for thickness 5-50 mm | Transverse |
-20 °C | 27 J Show Supplier Material materials with Energía de impacto Charpy of 27 J | min. | for thickness 50-70 mm | Transverse | |
-20 °C | 34 J Show Supplier Material materials with Energía de impacto Charpy of 34 J | min. | for thickness 5-50 mm | |
-20 °C | 34 J Show Supplier Material materials with Energía de impacto Charpy of 34 J | min. | for thickness 70-100 mm | Transverse | |
-20 °C | 41 J Show Supplier Material materials with Energía de impacto Charpy of 41 J | min. | for thickness 50-70 mm | |
-20 °C | 50 J Show Supplier Material materials with Energía de impacto Charpy of 50 J | min. | for thickness 70-100 mm | |
Límite elástico | 355 MPa Show Supplier Material materials with Límite elástico of 355 MPa | min. | for thickness 5-100 mm | Transverse | |
Resistencia a la tracción | 490 - 630 MPa Show Supplier Material materials with Resistencia a la tracción of 490 - 630 MPa | for thickness 5-100 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | min. |
Azufre | 0.035 % Show Supplier Material materials with Azufre of 0.035 % | max. |
Carbono | 0.18 % Show Supplier Material materials with Carbono of 0.18 % | max. |
Cobre | 0.35 % Show Supplier Material materials with Cobre of 0.35 % | max. |
Cromo | 0.2 % Show Supplier Material materials with Cromo of 0.2 % | max. |
Fósforo | 0.035 % Show Supplier Material materials with Fósforo of 0.035 % | max. |
Manganeso | 0.9 - 1.6 % Show Supplier Material materials with Manganeso of 0.9 - 1.6 % | |
Molibdeno | 0.08 % Show Supplier Material materials with Molibdeno of 0.08 % | max. |
Nitrógeno | 0.012 % Show Supplier Material materials with Nitrógeno of 0.012 % | max. |
Níquel | 0.4 % Show Supplier Material materials with Níquel of 0.4 % | max. |
Otro | 0.12 % Show Supplier Material materials with Otro of 0.12 % | max. | Nb + Ti + V |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Steel for shipbuilding can be used for the entire range of shipbuilding applications e.g. for the hull and interior of ships | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). | |
Other | Agreements The maximum thickness approved in shipbuilding specifications can be communicated on request by your sales agent. Available options Options available (after prior agreement): Mechanical properties Charpy V notch impact test specimens should be taken in the longitudinal direction. Transverse test specimens are not usually required. Transverse test results for plates and wide flats should be guaranteed by the supplier. |