General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 1.51 g/cm³ Show Supplier Material materials with Densidad of 1.51 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ISO 527-I |
Módulo elástico | 20.0 °C | 10 GPa Show Supplier Material materials with Módulo elástico of 10 GPa | ISO 527-I |
Resistencia a la flexión | 20.0 °C | 195 MPa Show Supplier Material materials with Resistencia a la flexión of 195 MPa | ISO 178 |
Resistencia a la tracción | 20.0 °C | 145 MPa Show Supplier Material materials with Resistencia a la tracción of 145 MPa | ISO 527-I |
Resistencia al choque, ensayo Charpy entallado | 20.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO 179-I |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75-I |
Technological properties
Property | ||
---|---|---|
Application areas | SKYi Stärk BH1118 is intended for injection moulding of highly demanding technical applications. The excellent properties of SKYi Stärk BH1118 make it suitable for: Electronic components, automotive parts, door handle, demanding components for various engineering sectors. SKYi Stärk BH1118 can, in many of these applications, substitute other engineering plastics or metal alloys. | |
Color | Available both in black and natural. | |
Other | Safety: SKYi Stärk BH1118 is not classified as a dangerous preparation. Dust and fines from the product may give a risk for dust explosion. All equipment should be properly earthed. Inhalation of dust may irritate the respiratory system and should be avoided. During processing of the product small amounts of fumes are generated, which require proper ventilation. Recycling: The product is suitable for recycling using modern methods of shredding and cleaning. Inhouse production waste should be kept clean to facilitate direct recycling. The Materials Safety Data Sheet is available on request. Please contact your SKYi representative for more details on various aspects of safety, recovery and disposal of the product. The following related documents are available on request, and represent various aspects on the usability, safety, recovery and disposal of the product. | |
Processing methods | Injection Molding: |