General
Property | Temperature | Value | |
---|---|---|---|
Densidad | 23.0 °C | 15.25 g/cm³ Show Supplier Material materials with Densidad of 15.25 g/cm³ | |
Aglutinante | Cobalt binder | ||
Estructura de grano | Ultrafine grain size |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell A | 23.0 °C | 94.5 [-] Show Supplier Material materials with Dureza Rockwell A of 94.5 [-] |
Dureza Vickers 10 | 23.0 °C | 2160 [-] Show Supplier Material materials with Dureza Vickers 10 of 2160 [-] |
Módulo elástico | 23.0 °C | 670 GPa Show Supplier Material materials with Módulo elástico of 670 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 7.8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 7.8 MPa·√m |
Resistencia a la compresión | 23.0 °C | 10400 MPa Show Supplier Material materials with Resistencia a la compresión of 10400 MPa |
Resistencia a la tracción transversal | 23.0 °C | 2900 MPa Show Supplier Material materials with Resistencia a la tracción transversal of 2900 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4.6E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.6E-6 1/K |
Conductividad térmica | 23.0 °C | 90 W/(m·K) Show Supplier Material materials with Conductividad térmica of 90 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobalto | 3 % Show Supplier Material materials with Cobalto of 3 % | as binder | |
Wolframio | WC balance |
Technological properties
Property |
---|