General
Property | Temperature | Value | |
---|---|---|---|
Densidad | 23.0 °C | 14.15 g/cm³ Show Supplier Material materials with Densidad of 14.15 g/cm³ | |
Estructura de grano | Fine (0,8µm - 1,3µm) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.22 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.22 [-] | |
Dureza Rockwell A | 23.0 °C | 89.5 [-] Show Supplier Material materials with Dureza Rockwell A of 89.5 [-] | |
Dureza Vickers 10 | 23.0 °C | 1310 [-] Show Supplier Material materials with Dureza Vickers 10 of 1310 [-] | EN ISO 6507-1 |
Dureza Vickers 30 | 23.0 °C | 1300 [-] Show Supplier Material materials with Dureza Vickers 30 of 1300 [-] | EN ISO 6507-1 |
Módulo elástico | 23.0 °C | 543 GPa Show Supplier Material materials with Módulo elástico of 543 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 15 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 15 MPa·√m | ISO 28079 |
Resistencia a la tracción transversal | 23.0 °C | 3500 MPa Show Supplier Material materials with Resistencia a la tracción transversal of 3500 MPa | DIN EN ISO 7438 |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 0.2 J/(kg·K) Show Supplier Material materials with Calor específico of 0.2 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 5.45E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.45E-6 1/K |
Conductividad térmica | 23.0 °C | 98 W/(m·K) Show Supplier Material materials with Conductividad térmica of 98 W/(m·K) |
Difusividad térmica | 23.0 °C | 34.4 mm²/s Show Supplier Material materials with Difusividad térmica of 34.4 mm²/s |
Chemical properties
Technological properties
Property |
---|