General
Property | Temperature | Value | |
---|---|---|---|
Densidad | 23.0 °C | 14.7 g/cm³ Show Supplier Material materials with Densidad of 14.7 g/cm³ | |
Estructura de grano | Submicron (0,5µm - 0,8µm) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.21 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.21 [-] | |
Dureza Rockwell A | 23.0 °C | 92.8 [-] Show Supplier Material materials with Dureza Rockwell A of 92.8 [-] | |
Dureza Vickers 10 | 23.0 °C | 1780 [-] Show Supplier Material materials with Dureza Vickers 10 of 1780 [-] | EN ISO 6507-1 |
Dureza Vickers 30 | 23.0 °C | 1750 [-] Show Supplier Material materials with Dureza Vickers 30 of 1750 [-] | EN ISO 6507-1 |
Módulo elástico | 23.0 °C | 605 GPa Show Supplier Material materials with Módulo elástico of 605 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 9.5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9.5 MPa·√m | ISO 28079 |
Resistencia a la tracción transversal | 23.0 °C | 3700 MPa Show Supplier Material materials with Resistencia a la tracción transversal of 3700 MPa | DIN EN ISO 7438 |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 0.2 J/(kg·K) Show Supplier Material materials with Calor específico of 0.2 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 4.95E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.95E-6 1/K |
Conductividad térmica | 23.0 °C | 66 W/(m·K) Show Supplier Material materials with Conductividad térmica of 66 W/(m·K) |
Difusividad térmica | 23.0 °C | 22.8 mm²/s Show Supplier Material materials with Difusividad térmica of 22.8 mm²/s |
Chemical properties
Technological properties
Property |
---|