General
Property | Temperature | Value | |
---|---|---|---|
Densidad | 23.0 °C | 14.1 g/cm³ Show Supplier Material materials with Densidad of 14.1 g/cm³ | |
Estructura de grano | Ultrafine (0,2µm - 0,5µm) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.22 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.22 [-] | |
Dureza Rockwell A | 23.0 °C | 92.7 [-] Show Supplier Material materials with Dureza Rockwell A of 92.7 [-] | |
Dureza Vickers 10 | 23.0 °C | 1760 [-] Show Supplier Material materials with Dureza Vickers 10 of 1760 [-] | EN ISO 6507-1 |
Dureza Vickers 30 | 23.0 °C | 1730 [-] Show Supplier Material materials with Dureza Vickers 30 of 1730 [-] | EN ISO 6507-1 |
Módulo elástico | 23.0 °C | 549 GPa Show Supplier Material materials with Módulo elástico of 549 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 9.8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9.8 MPa·√m | ISO 28079 |
Resistencia a la tracción transversal | 23.0 °C | 4600 MPa Show Supplier Material materials with Resistencia a la tracción transversal of 4600 MPa | DIN EN ISO 7438 |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 0.21 J/(kg·K) Show Supplier Material materials with Calor específico of 0.21 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 5.4E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.4E-6 1/K |
Conductividad térmica | 23.0 °C | 51 W/(m·K) Show Supplier Material materials with Conductividad térmica of 51 W/(m·K) |
Difusividad térmica | 23.0 °C | 17.6 mm²/s Show Supplier Material materials with Difusividad térmica of 17.6 mm²/s |
Chemical properties
Technological properties
Property |
---|