Property | Value |
---|---|
Área superficial específica | 7 - 15 m²/g Show Supplier Material materials with Área superficial específica of 7 - 15 m²/g |
Technological properties
Property | ||
---|---|---|
Application areas | solid oxide fuel cell, SOFC, solid oxide electolyzer cell, SOEC, membranes for hydrogen separation, protonic conductor, tubular ceramic fuel cell, composite electrode, cathode, electrolyte, catalyst | |
Chemical composition | BaZr0.7Ce0.1Y0.1Yb0.1O3, BaZr0.4Ce0.4Y0.1Yb0.1O3 | |
Color | Fine, white powder | |
Processing history | Cerpotech applies spray pyrolysis, a soft chemistry technique with a great potential, to produce high quality, multi-component ceramic oxide powders. With this aqueous-based environmentally friendly technology, Cerpotech is able to offer fine complex ceramic oxide powders of tailored compositions with high phase purity, high chemical purity, very high homogeneity, narrow particle distribution, offering excellent properties for further processing at competetive prices. |