General
Property | Value | Comment | |
---|---|---|---|
Carbon equivalent (CEV) | 0.39 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.39 [-] | max. value for plate thickness 10 to 40 mm | |
Carbon equivalent note | CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Cu+Ni)/15 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -50 °C | 80 J Show Supplier Material materials with Charpy impact energy, V-notch of 80 J | average of 3 tests | longitudinal/transverse specimens | no individual value is to be less than 70% of the specified minimum |
Elongación | 20 % Show Supplier Material materials with Elongación of 20 % | min. for plate thickness 10 to 40 mm, A5 | |
28 % Show Supplier Material materials with Elongación of 28 % | min. for plate thickness 10 to 40 mm, A2 | ||
Límite elástico | 420 MPa Show Supplier Material materials with Límite elástico of 420 MPa | min. ReH for plate thickness 10 to 40 mm | |
Resistencia a la tracción | 500 - 660 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 660 MPa | for plate thickness 10 to 40 mm |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.02 - 0.06 % Show Supplier Material materials with Aluminio of 0.02 - 0.06 % | ||
Azufre | 0.0013 % Show Supplier Material materials with Azufre of 0.0013 % | max. | |
Carbono | 0.06 % Show Supplier Material materials with Carbono of 0.06 % | max. | |
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % | max. | |
Cromo | 0.25 % Show Supplier Material materials with Cromo of 0.25 % | max. | |
Fósforo | 0.015 % Show Supplier Material materials with Fósforo of 0.015 % | max. | |
Hierro | Balance | ||
Manganeso | 1 - 1.6 % Show Supplier Material materials with Manganeso of 1 - 1.6 % | ||
Molibdeno | 0.08 % Show Supplier Material materials with Molibdeno of 0.08 % | max. | |
Niobio | 0.05 % Show Supplier Material materials with Niobio of 0.05 % | max. | |
Nitrógeno | 0.01 % Show Supplier Material materials with Nitrógeno of 0.01 % | max. | |
Níquel | 0.3 % Show Supplier Material materials with Níquel of 0.3 % | max. | |
Silicona | 0.15 - 0.5 % Show Supplier Material materials with Silicona of 0.15 - 0.5 % | ||
Titanio | 0.02 % Show Supplier Material materials with Titanio of 0.02 % | max. | |
Vanadio | 0.08 % Show Supplier Material materials with Vanadio of 0.08 % | max. |
Technological properties
Property | ||
---|---|---|
Cold Forming | DI-TANK 420 can generally be well cold formed with regard to its high toughness, i.e. formed at temperatures below 580 °C. Cold forming is always related to a hardening of the steel and to a decrease in toughness. This change in the mechanical and HIC properties can, as a rule, be partially recovered through a subsequent stress relief heat treatment at a temperature below 580 °C. When DI-TANK 420 HIC is cold formed more than 5% a subsequent stress relief heat treatment is necessary. Irregularities at the flame cut or sheared edges in the bending area should be ground before cold forming. For larger cold forming amounts we recommend you to consult us prior to ordering. | |
Delivery condtion | DITANK420: Thermo-mechanical rolling according to EN 10028-5 (M) or thermo-mechanical control process according to A/SA841, A/SA841M (TMCP). | |
Flame cutting and welding | DI-TANK 420 can be flame cut in all thickness ranges without preheating due to its low hardenability. Plasma and laser cutting can also be carried out without preheating for typical thickness. The family of DI-TANK has an excellent weldability if the general technical rules are observed (EN 1011 has to be applied analogously). The risk of cold cracking is low, so a preheating may not be necessary for most of the welds. When welding thicker plates preheating can still be avoided if filler materials and welding conditions are applied that lead to a very low hydrogen transfer (up to 5 ml/100 g DM according to ISO 3690). The low contents of carbon and other alloy elements lead to favourable toughness properties in the heat-affected-zone, even with relatively high heat inputs. Depending on the chosen welding process, welding filler material as well as toughness requirements in the heat affected zone, also it permits t8/5 cooling times above of 25 s as stated in EN 1011-2. The upper limit of heat input is however dependent from the toughness requirements in particular the impact test temperature. | |
General note | A stress relief heat treatment may be required above 580 °C by the API 650, API 620 and also EN 14620. The standards authorize a reduction of the PWHT temperature (below 580 °C) providing a longer holding time, with the purchaser’s agreement. Then, the parameters of the PWHT have to be specified and agreed at the time of the inquiry. Nevertheless, DI-TANK 420 is offered with a HP value (Pcrit) of 17.6. If special requirements which are not listed in this material data sheet, are to be met by the steel due to its intended use or processing, these requirements are to be agreed before placing the order. The information in this data sheet is a product description. This data sheet is updated as occasion demands. The latest version is available from the mill or as download at www.dillinger.de. | |
Hot forming | Hot forming, i.e. forming at temperatures above 580 °C, leads to changes in the original material condition. It is impossible to re-establish the same material properties that had been achieved during the original manufacture through a further heat treatment. Therefore hot forming is not permitted. The same limitation applies for heat treatments. | |
Hydrogen induced cracking | The HIC test is performed by the test house of Dillinger. Unless otherwise agreed, one set of tests is carried out per heat. Test procedure in accordance with NACE TM 0284: The inspection test is performed in accordance with NACE TM 0284: a set of three specimens with defined dimensions are immersed for 96 h in a solution saturated with hydrogen sulfide. In general the test is performed with test solution A. Test solution A contains 5 % sodium chloride with 0.5 % acetic acid. It has a pH of 2.6 – 2.8 before saturation with hydrogen sulfide and a pH ≤ 4.0 at the end of the test. Crack evaluation in accordance with NACE TM 0284: When the immersion is finished the specimens are cut to perform metallographic crack evaluation on 3 sections of each specimen. The crack dimensions are put in proportion to the sections’ dimensions and are described by CLR (crack length ratio), CTR (crack thickness ratio) and CSR (crack sensitivity ratio) values. The test result and acceptance criteria are average values (3 sections) of CLR, CTR and CSR. | |
Other | In addition to the marking required by the product specification, at least the following information will be marked, with low stress steel stamps: | |
Processing history | BOF-converter process and metallurgical ladle treatment. The steel is fully killed and fine grained by the addition of nitrogen fixing elements. In order to achieve the defined HIC resistance of DI-TANK 420 HIC the following specific production process route is applied: Only the combination of the above mentioned measures and the quality assurance adapted to HIC resistant steel assure that the specified HIC resistance is obtained. This is also stated in the inspection certificate. | |
Processing methods | The customer is responsible for the selection of the material. The entire processing and application techniques are of fundamental importance to the reliability of the products made from steel. The user should ensure that his design, calculation and processing methods are aligned with the material, correspond to the state-of-the-art that fabricator has to comply with and are suitable for the intended use. The recommendations given in EN 1011-2 should be observed. | |
Surface condition | Unless otherwise agreed, the provisions in accordance with class B2 of EN 10163-2 in case of ordering the P420ML2 variant, otherwise in accordance with ASTM-A20 in case of ordering the A/SA841(M)-grade B class 2 variant, are applicable. | |
Testings | Tensile test and impact tests are carried out according to the relevant standards. Unless otherwise agreed, the impact test will be performed at -50 °C on transverse test pieces. | |
Tolerances | Unless otherwise agreed, the tolerances for the thickness in accordance with class B of EN 10029 in case of ordering the P420ML2 variant, otherwise in accordance with ASTM-A20 in case of ordering the A/SA841(M)-grade B class 2 variant, are applicable. |