General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.06 % Show Supplier Material materials with Absorción de agua of 0.06 % | ISO 62, 100°C/30 min |
Densidad | 23.0 °C | 1.95 g/cm³ Show Supplier Material materials with Densidad of 1.95 g/cm³ | DIN 53479 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.4 % Show Supplier Material materials with Elongación of 1.4 % | ISO 178 |
Módulo elástico | 23.0 °C | 17 GPa Show Supplier Material materials with Módulo elástico of 17 GPa | ISO 178 (Flexural Test) |
Resistencia a la flexión | 23.0 °C | 190 MPa Show Supplier Material materials with Resistencia a la flexión of 190 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la tracción of 100 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 22 kJ/m² | ISO 179-1 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2E-5 1/K | ISO 11359-2, Mean value for 20-105°C |
Conductividad térmica | 23.0 °C | 0.85 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.85 W/(m·K) | ISO 8894 |
Temperatura de transición del vidrio | 120 °C Show Supplier Material materials with Temperatura de transición del vidrio of 120 °C | ISO 6721-7 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5 [-] | IEC 60250 |
Loss tangent, 50Hz | 23.0 °C | 1.6 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.6 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 300 V Show Supplier Material materials with Índice de seguimiento comparativo of 300 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Encapsulation of electrical devices, e.g. Electronic, Sensors, Solenoids, Stators | |
Fillers | Glass Fiber |