Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.7 % Show Supplier Material materials with Elongación of 1.7 % | ISO 178 |
Módulo elástico | 23.0 °C | 12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | ISO 178 (Flexural Test) |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 11 kJ/m² | ISO 179-1 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.1E-5 1/K | ISO 11359-2, Mean value for 20-105°C |
Conductividad térmica | 23.0 °C | 0.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.7 W/(m·K) | ISO 8894 |
Temperatura de transición del vidrio | 110 °C Show Supplier Material materials with Temperatura de transición del vidrio of 110 °C | ISO 6721-7 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5.8 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5.8 [-] | IEC 60250 |
Loss tangent, 50Hz | 23.0 °C | 1.3 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.3 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 18 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18 kV/mm | IEC 60243-1, 3mm Plate |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 375 V Show Supplier Material materials with Índice de seguimiento comparativo of 375 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | Encapsulation of electrical devices e.g. solenoids, stators, transformers, electronic | |
Fillers | Glass Fiber |