General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | ISO 62, 100°C/30 min |
Densidad | 23.0 °C | 2.25 g/cm³ Show Supplier Material materials with Densidad of 2.25 g/cm³ | DIN 53479 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 0.8 % Show Supplier Material materials with Elongación of 0.8 % | ISO 178 |
Módulo elástico | 23.0 °C | 18 GPa Show Supplier Material materials with Módulo elástico of 18 GPa | ISO 178 (Flexural Test) |
Resistencia a la flexión | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la flexión of 125 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | ISO 527 |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 8 kJ/m² | ISO 179-1 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | TMA |
Conductividad térmica | 23.0 °C | 1.4 W/(m·K) Show Supplier Material materials with Conductividad térmica of 1.4 W/(m·K) | ISO 8894 |
Temperatura de transición del vidrio | 160 °C Show Supplier Material materials with Temperatura de transición del vidrio of 160 °C | ISO 6721 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5.8 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5.8 [-] | IEC 60250 |
Loss tangent, 50Hz | 23.0 °C | 1.5 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.5 [-] | IEC 60250 |
Rigidez dieléctrica | 23.0 °C | 19 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 19 kV/mm | IEC 60243-1, 3mm Plate |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 425 V Show Supplier Material materials with Índice de seguimiento comparativo of 425 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Application areas | For applications with high heat dissipation e.g. electronic coatings, rotors, stators etc. |