General
Property | Value |
---|---|
Densidad | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ |
Mecánica
Property | Value | Testing Standard |
---|---|---|
Elongación | 35 % Show Supplier Material materials with Elongación of 35 % | DIN EN ISO 527-1 |
Módulo elástico | 1.4 GPa Show Supplier Material materials with Módulo elástico of 1.4 GPa | DIN EN ISO 527-1 |
Resistencia a la tracción | 16 MPa Show Supplier Material materials with Resistencia a la tracción of 16 MPa | DIN EN ISO 527-1 |
Resistencia al choque, ensayo Charpy no entallado | 115 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 115 kJ/m² | DIN EN ISO 179-1eU |
Aplicaciones térmicas
Property | Value | Testing Standard | Comment |
---|---|---|---|
Temperatura de fusión | 165 °C Show Supplier Material materials with Temperatura de fusión of 165 °C | DIN 53765 | |
Temperatura de transición del vidrio | -8 °C Show Supplier Material materials with Temperatura de transición del vidrio of -8 °C | ||
Temperatura máx. de funcionamiento | 100 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 100 °C | Long | |
130 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 130 °C | Short |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Velocidad de flujo de la masa derretida | 11 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 11 g/10min | DIN EN ISO 1133 | 230°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Certifications | Explanation of food contact according to FDA and EU 10/2011 on request | |
Color | Blue | |
Detectability | Inductive: 6 mm Al | |
Fillers | Detectable Filler | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 100, drying time (h): 2, mould temperature (°C): 100, material temperature (°C): 250, cylinder/processing temperature (°C): 260 |