General
Property | Value |
---|---|
Densidad | 6.5 g/cm³ Show Supplier Material materials with Densidad of 6.5 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Carga límite de trabajo | 370 MPa Show Supplier Material materials with Carga límite de trabajo of 370 MPa | |
450 MPa Show Supplier Material materials with Carga límite de trabajo of 450 MPa | ||
Dureza Vickers | 280 - 320 [-] Show Supplier Material materials with Dureza Vickers of 280 - 320 [-] | HV 0.5 |
Elongación | 2.8 % Show Supplier Material materials with Elongación of 2.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical, Aerospace, Biomedical | |
Other | Diameter 10 mm by 2-7 mm disks. Diameter 15 mm by 2-7 mm disks. 20 x 10 x 2 to 8 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |