General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | ISO 1183 |
Water content | 23.0 °C | 0.1 % Show Supplier Material materials with Water content of 0.1 % | ISO 15512 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % | min., ISO 527-2 (5mm/min) | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 (2mm/min) | ||
Módulo elástico | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | ISO 527-2 (1mm/min) | ||
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 (2mm/min) | ||
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | ISO 527-2 (5mm/min) | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA | ||
23.0 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod entallado | -40.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | ||
23.0 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 13 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Charpy no entallado | no break at 23°C; ISO 179/1eU | ||||
Resistencia al choque, ensayo Izod no entallado | no break at 23°C; ISO 180/1U |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 190 °C | ISO 75-2/B | |
Heat deflection temperature, 1.80 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C | ISO 75-2/A | |
Temperatura de fusión | 260 °C Show Supplier Material materials with Temperatura de fusión of 260 °C | ISO 3146 | |
Inflamabilidad | UL94 (0.8mm) HB |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+14 Ω/sq | ASTM D257 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | EN 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Halogen free based on red phosphorus flame retardant grades, compliance with RoHS derivatives, with rating UL94 V0 and glow-wire at 960°C, which is used in many sectors of industy and has excellent mechanical properties. | |
Certifications | RoHS | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |