General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4 % Show Supplier Material materials with Elongación of 4 % | ISO 527-2 (5mm/min) |
Módulo de flexión | 23.0 °C | 3.5 GPa Show Supplier Material materials with Módulo de flexión of 3.5 GPa | ISO 178 (2mm/min) |
Módulo elástico | 23.0 °C | 3.8 GPa Show Supplier Material materials with Módulo elástico of 3.8 GPa | ISO 527-2 (1mm/min) |
Resistencia a la flexión | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la flexión of 105 MPa | ISO 178 (2mm/min) |
Resistencia a la tracción | 23.0 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | ISO 527-2 (5mm/min) |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 30 kJ/m² | ISO 179/1eU |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 3 kJ/m² | ISO 180/1A |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 25 kJ/m² | ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 20 % Show Supplier Material materials with Contenido de cenizas of 20 % | ISO 3451-4 | ||
Heat deflection temperature, 0.45 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C | ISO 75-2/B | |||
Heat deflection temperature, 1.80 MPa | 75 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 75 °C | ISO 75-2/A | |||
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | ISO 3146 | |||
Inflamabilidad | UL94 (0.8mm) HB |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | ASTM D257 |
Índice de seguimiento comparativo | 23.0 °C | 250 V Show Supplier Material materials with Índice de seguimiento comparativo of 250 V | EN 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | EPIMIX PBT glass bead reinforced grades are used in all sectors of industry, has and excellent surface finish, low warpage and all around excellent mechanical properties. | |
Fillers | 20% Glass Bead | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |