General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Densidad of 1.3 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 8 % Show Supplier Material materials with Elongación of 8 % | ISO 527-2 (5mm/min) |
Módulo de flexión | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ISO 178 (2mm/min) |
Módulo elástico | 23.0 °C | 2.7 GPa Show Supplier Material materials with Módulo elástico of 2.7 GPa | ISO 527-2 (1mm/min) |
Resistencia a la flexión | 23.0 °C | 85 MPa Show Supplier Material materials with Resistencia a la flexión of 85 MPa | ISO 178 (2mm/min) |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | ISO 527-2 (5mm/min) |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 75 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 75 kJ/m² | ISO 179/1eU |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 7 kJ/m² | ISO 180/1A |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 70 kJ/m² | ISO 180/1U |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 160 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 160 °C | ISO 75-2/B | |
Heat deflection temperature, 1.80 MPa | 60 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 60 °C | ISO 75-2/A | |
Temperatura de fusión | 225 °C Show Supplier Material materials with Temperatura de fusión of 225 °C | ISO 3146 | |
Inflamabilidad | UL94 (0.8mm) HB |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq | ASTM D257 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | EN 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | EPIMIX PBT is used in all sectors of industry, has and excellent surface finish, low warpage and all around excellent mechanical properties. EPIMIX PBT is approved for applications in direct contact with drinking water and food. | |
Certifications | Drinking Water,Food Contact | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |