General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.26 g/cm³ Show Supplier Material materials with Densidad of 3.26 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.25 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.25 [-] |
Módulo elástico | 23.0 °C | 300 GPa Show Supplier Material materials with Módulo elástico of 300 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 7.5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 7.5 MPa·√m |
Resistencia a la flexión | 23.0 °C | 750 MPa Show Supplier Material materials with Resistencia a la flexión of 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.5E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5E-6 1/K | |
1000.0 °C | 3.2E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.2E-6 1/K | ||
Conductividad térmica | 23.0 °C | 85 W/(m·K) Show Supplier Material materials with Conductividad térmica of 85 W/(m·K) | |
Parámetro de choque térmico (R1) | 586 °C Show Supplier Material materials with Parámetro de choque térmico (R1) of 586 °C | ||
Parámetro de choque térmico (R2) | 49805 W/m Show Supplier Material materials with Parámetro de choque térmico (R2) of 49805 W/m | ||
Temperatura máx. de funcionamiento | 1500 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1500 °C | in inert gas | |
Temperatura máx. de funcionamiento, largo | 1300 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, largo of 1300 °C | in air |