General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.55 g/cm³ Show Supplier Material materials with Densidad of 3.55 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.26 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.26 [-] |
Módulo elástico | 23.0 °C | 310 GPa Show Supplier Material materials with Módulo elástico of 310 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 6 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 MPa·√m |
Resistencia a la flexión | 23.0 °C | 720 MPa Show Supplier Material materials with Resistencia a la flexión of 720 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.9E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.9E-6 1/K | |
Conductividad térmica | 23.0 °C | 21 W/(m·K) Show Supplier Material materials with Conductividad térmica of 21 W/(m·K) | |
Temperatura máx. de funcionamiento | 1000 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1000 °C | in inert gas | |
Temperatura máx. de funcionamiento, largo | 800 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, largo of 800 °C | in air |