General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.14 g/cm³ Show Supplier Material materials with Densidad of 3.14 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.16 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.16 [-] |
Módulo elástico | 23.0 °C | 400 GPa Show Supplier Material materials with Módulo elástico of 400 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 3 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3 MPa·√m |
Resistencia a la flexión | 23.0 °C | 550 MPa Show Supplier Material materials with Resistencia a la flexión of 550 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 3.3E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.3E-6 1/K | |
1000.0 °C | 4.6E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.6E-6 1/K | ||
Conductividad térmica | 23.0 °C | 125 W/(m·K) Show Supplier Material materials with Conductividad térmica of 125 W/(m·K) | |
Parámetro de choque térmico (R1) | 251 °C Show Supplier Material materials with Parámetro de choque térmico (R1) of 251 °C | ||
Parámetro de choque térmico (R2) | 31386 W/m Show Supplier Material materials with Parámetro de choque térmico (R2) of 31386 W/m | ||
Temperatura máx. de funcionamiento | 1900 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1900 °C | in inert gas | |
Temperatura máx. de funcionamiento, largo | 1600 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, largo of 1600 °C | in air |