General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 6.1 g/cm³ Show Supplier Material materials with Densidad of 6.1 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.3 [-] |
Módulo elástico | 23.0 °C | 490 GPa Show Supplier Material materials with Módulo elástico of 490 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 MPa·√m |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 5.9E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.9E-6 1/K | |
1000.0 °C | 6.4E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.4E-6 1/K | ||
Conductividad térmica | 23.0 °C | 23 W/(m·K) Show Supplier Material materials with Conductividad térmica of 23 W/(m·K) | |
Temperatura máx. de funcionamiento | 2200 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 2200 °C | in inert gas | |
Temperatura máx. de funcionamiento, largo | 500 °C Show Supplier Material materials with Temperatura máx. de funcionamiento, largo of 500 °C | in air |