General
Property | Value | Comment |
---|---|---|
Bio-based content | 20 % Show Supplier Material materials with Bio-based content of 20 % | |
50 % Show Supplier Material materials with Bio-based content of 50 % | ||
Densidad | 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.17 g/cm³ | Calculated |
Mecánica
Property | Value | Comment |
---|---|---|
Módulo de flexión | 0.618 GPa Show Supplier Material materials with Módulo de flexión of 0.618 GPa | ASTM D790 |
Módulo elástico | 0.65 GPa Show Supplier Material materials with Módulo elástico of 0.65 GPa | ASTM D638 |
Resistencia a la flexión | 25 MPa Show Supplier Material materials with Resistencia a la flexión of 25 MPa | ASTM D790 |
Resistencia a la tracción | 16 MPa Show Supplier Material materials with Resistencia a la tracción of 16 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 130 °C Show Supplier Material materials with Temperatura de fusión of 130 °C | ASTM D3418 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 1.3 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 1.3 g/10min | ASTM D1238 (190°C/10 kg) |
Technological properties
Property | ||
---|---|---|
Application areas | BioBlend® XD 22620 is designed for blow molding applications that require stress crack resistance, rigidity, and high impact strength. | |
Certifications | USDA Certified Bio-based product |