Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Supplier Material materials with Aluminio of 0.05 % |
Arsénico | 0.02 - 0.15 % Show Supplier Material materials with Arsénico of 0.02 - 0.15 % |
Cobre | 61 - 63 % Show Supplier Material materials with Cobre of 61 - 63 % |
Estaño | 0.1 % Show Supplier Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Supplier Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Supplier Material materials with Níquel of 0.3 % |
Plomo | 1.7 - 2.8 % Show Supplier Material materials with Plomo of 1.7 - 2.8 % |
Zinc | Balance, REM |