Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 1.3 % Show Supplier Material materials with Aluminio of 0.3 - 1.3 % |
Cobre | 59 - 61.5 % Show Supplier Material materials with Cobre of 59 - 61.5 % |
Estaño | 0.3 % Show Supplier Material materials with Estaño of 0.3 % |
Hierro | 1 % Show Supplier Material materials with Hierro of 1 % |
Manganeso | 0.6 - 1.8 % Show Supplier Material materials with Manganeso of 0.6 - 1.8 % |
Níquel | 0.6 % Show Supplier Material materials with Níquel of 0.6 % |
Plomo | 1 % Show Supplier Material materials with Plomo of 1 % |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Zinc | Balance, REM |