Chemical properties
Property | Value |
---|---|
Aluminio | 5 - 6 % Show Supplier Material materials with Aluminio of 5 - 6 % |
Cobre | 63 - 65 % Show Supplier Material materials with Cobre of 63 - 65 % |
Estaño | 0.2 % Show Supplier Material materials with Estaño of 0.2 % |
Hierro | 2 - 3.5 % Show Supplier Material materials with Hierro of 2 - 3.5 % |
Manganeso | 3.5 - 5 % Show Supplier Material materials with Manganeso of 3.5 - 5 % |
Níquel | 0.5 % Show Supplier Material materials with Níquel of 0.5 % |
Plomo | 0.2 - 0.8 % Show Supplier Material materials with Plomo of 0.2 - 0.8 % |
Silicona | 0.2 % Show Supplier Material materials with Silicona of 0.2 % |
Zinc | Balance, REM |