Chemical properties
Property | Value |
---|---|
Aluminio | 4 - 5 % Show Supplier Material materials with Aluminio of 4 - 5 % |
Cobre | 65 - 68 % Show Supplier Material materials with Cobre of 65 - 68 % |
Estaño | 0.2 % Show Supplier Material materials with Estaño of 0.2 % |
Hierro | 0.5 - 3 % Show Supplier Material materials with Hierro of 0.5 - 3 % |
Manganeso | 0.5 - 3 % Show Supplier Material materials with Manganeso of 0.5 - 3 % |
Níquel | 1 % Show Supplier Material materials with Níquel of 1 % |
Plomo | 0.2 - 0.8 % Show Supplier Material materials with Plomo of 0.2 - 0.8 % |
Zinc | Balance, REM |