General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 3.17 g/cm³ Show Supplier Material materials with Densidad of 3.17 g/cm³ |
Densidad aparente | 23.0 °C | 0.85 g/cm³ Show Supplier Material materials with Densidad aparente of 0.85 g/cm³ |
Rango de tamaño de partículas | 100 µm Show Supplier Material materials with Rango de tamaño de partículas of 100 µm |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 26 GPa Show Supplier Material materials with Módulo elástico of 26 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 4 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 4 MPa·√m |
Resistencia a la flexión | 23.0 °C | 500 MPa Show Supplier Material materials with Resistencia a la flexión of 500 MPa |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Flujo de Hall | 23.0 °C | 22.5 s/50g Show Supplier Material materials with Flujo de Hall of 22.5 s/50g |
Technological properties
Property | ||
---|---|---|
Application areas | Silicon Carbide Ready-To-Press granules for solid-state (SSiC) sintered technical ceramics. | |
Chemical composition | Sinter additives: Carbon (Resin), Boron Carbide; Binder: 9,5%; Moisture Content: 0,6%; SiC type balance: SINTEX 15 C |