General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 16.8 - 17.6 g/cm³ Show Supplier Material materials with Densidad of 16.8 - 17.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 23.0 °C | 250 - 290 [-] Show Supplier Material materials with Dureza Vickers 10 of 250 - 290 [-] |
Resistencia a la tracción | 23.0 °C | 680 - 820 MPa Show Supplier Material materials with Resistencia a la tracción of 680 - 820 MPa |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.80E+7 - 2.20E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.80E+7 - 2.20E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 2E-3 % Show Supplier Material materials with Aluminio of 2E-3 % | Max. | |
Arsénico | 2E-3 % Show Supplier Material materials with Arsénico of 2E-3 % | Max. | |
Azufre | 2E-3 % Show Supplier Material materials with Azufre of 2E-3 % | Max. | |
Calcio | 2E-3 % Show Supplier Material materials with Calcio of 2E-3 % | Max. | |
Carbono | 5E-3 % Show Supplier Material materials with Carbono of 5E-3 % | Max. | |
Cobalto | 3E-3 % Show Supplier Material materials with Cobalto of 3E-3 % | Max. | |
Cobre | 8 - 12 % Show Supplier Material materials with Cobre of 8 - 12 % | ||
Cromo | 2E-3 % Show Supplier Material materials with Cromo of 2E-3 % | Max. | |
Hierro | 3E-3 % Show Supplier Material materials with Hierro of 3E-3 % | Min. | |
Magnesio | 2E-3 % Show Supplier Material materials with Magnesio of 2E-3 % | Max. | |
Molibdeno | 5E-3 % Show Supplier Material materials with Molibdeno of 5E-3 % | Min. | |
Níquel | 0.5 % Show Supplier Material materials with Níquel of 0.5 % | Max. | |
Potasio | 1E-3 % Show Supplier Material materials with Potasio of 1E-3 % | Max. | |
Silicona | 3E-3 % Show Supplier Material materials with Silicona of 3E-3 % | Max. | |
Sodio | 2E-3 % Show Supplier Material materials with Sodio of 2E-3 % | Max. | |
Wolframio | balance |
Technological properties
Property | ||
---|---|---|
Application areas | EDM electrode material for spark erosion; Resistance and contact welding electrode material; Contact material for electrical engineering; Material to balance rotating systems |