A high quality aerospace grade aluminum alloy (6061B) reinforced with 20 vol.% silicon carbide particles which produces a metal matrix composite (MMC). 620XF is manufactured via a powder metallurgy route using a mechanical alloying process to ensure a homogeneous reinforcement distribution, providing a refined grain structure enhancing mechanical properties. The MMC is heat treatable offering high strength and modulus for structural applications and is available in billet, forged and extruded forms.


620XF Advantages:


  • Precision section extrusion using standard dies
  • Reduced wall thickness offering weight saving
  • High stiffness and strength
  • Robust and ductile for damage resistance
  • Good corrosion and fatigue performance
  • Thermally stable
  • Equivalent Materials

    Los datos sobre este material han sido proporcionados por Materion Brush GmbH.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyTemperatureValue

    Densidad

    23.0 °C

    2.8 g/cm³

    Show Supplier Material materials with Densidad of 2.8 g/cm³

    Mecánica

    PropertyTemperatureValue

    Coeficiente de Poisson

    23.0 °C

    0.3 [-]

    Show Supplier Material materials with Coeficiente de Poisson of 0.3 [-]

    Elongación

    23.0 °C

    7 %

    Show Supplier Material materials with Elongación of 7 %

    Límite elástico Rp 0,2

    23.0 °C

    380 MPa

    Show Supplier Material materials with Límite elástico Rp 0,2 of 380 MPa

    Módulo elástico

    23.0 °C

    103 GPa

    Show Supplier Material materials with Módulo elástico of 103 GPa

    Resistencia a la tracción

    23.0 °C

    470 MPa

    Show Supplier Material materials with Resistencia a la tracción of 470 MPa

    Aplicaciones térmicas

    PropertyTemperatureValue

    Calor específico

    23.0 °C

    850 J/(kg·K)

    Show Supplier Material materials with Calor específico of 850 J/(kg·K)

    Coeficiente de dilatación térmica

    23.0 °C

    1.7E-5 1/K

    Show Supplier Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K

    Conductividad térmica

    23.0 °C

    150 W/(m·K)

    Show Supplier Material materials with Conductividad térmica of 150 W/(m·K)

    Temperatura de fusión

    570 °C

    Show Supplier Material materials with Temperatura de fusión of 570 °C

    Technological properties

    Property
    Application areas

    Commercial and Military Aerospace: Outlet guide vanes, Hydraulic / Fuel blocks, Wheels, Fixed wing structure/ skins, Helicopter components - Commercial and Preformance Automotive: Pistons, Piston pins, Cylinder liners, Brake calipers, Connecting rods, Push rods, Valve train, Chassis components - Space, Defence and Optical Systems: Optical systems & sensors, Satellite structures, Astronomical telescopes

    Processing history